UNS R30605

High-strength; resists oxidation and carburization up to 1900° F.  Resists galling, acids and body fluids.  At certain concentrations, will resist hydrochloric and nitric acid.  Resistant to wet chlorine environments at room temperature. Widely used in gas turbine engine components, bearings, springs, marine environments and heart valves.

Haynes® 25 Fact Sheet 

Composition[Co rem(50%), Cr 19-21%, W 14-16%, Ni 9-11%, Fe 3%max, Mn 2%max]
SpecificationsASTM F90, AMS 5796
Density0.330 lbs/in³
Tensile Strength180 Kpsi*
Elongation45%*
Melt2425° F
Max. Operating Temperature1800-2000° F

* Tensile strength and elongation are for annealed 0.012″ wire diameter. Please note that material performance data is provided a reference guide only… There are many factors involved in wire cloth performance, so please consult with an experienced engineer before choosing the metal best suited for your unique needs!

Haynes 25 is a registered trademark of Haynes International, Inc.