USN N10276

Particularly suitable for use in corrosive environments where reducing and oxidizing are common.  Resists localized attack, pitting and stress corrosion cracking.  In wide use in the pulp and paper industries, as well as pollution control and chemical processing.

Hastelloy® C-276 Fact Sheet

Composition[Ni 57%, Mo 16%, Cr 15.5%, Fe 5.5%]
SpecificationsASTM B574
Density0.321 lbs/in³
Tensile Strength142 Kpsi*
Elongation48%*
Melt2500° F
Max. Operating Temperature1800° F

* Tensile strength and elongation are for annealed 0.012″ wire diameter. Please note that material performance data is provided a reference guide only… There are many factors involved in wire cloth performance, so please consult with an experienced engineer before choosing the metal best suited for your unique needs!