| degrees Fahrenheit | degrees Celsius | Use |
| 15 to 0 | -18 to -9.5 | Deep Freeze |
| 32 to 100 | 0 to 38 | Quench |
| 70 to 200 | 21 to 93 | Washing |
| 200 to 500 | 93 to 260 | Baking |
| 200 to 600 | 93 to 315 | Drying |
| 300 to 1100 | 149 to 593 | Tempering |
| 750 to 1050 | 400 to 560 | Glass Annealing |
| 1150 to 1300 | 600 to 704 | Glass Decorating -- Strain Relieving |
| 1150 to 1450 | 600 to 800 | Brass and Copper Annealing |
| 1350 to 1700 | 730 to 926 | Silver Brazing |
| 1400 to 1700 | 760 to 926 | Hardening and Carburizing |
| 1600 to 1900 | 871 to 1036 | Controlled Atmosphere Annealing -- Normalizing |
| 1650 to 1750 | 880 to 960 | Vitreous Enameling |
| 1600 to 1900 | 871 to 1036 | Powder Metallurgy |
| 1900 to 2200 | 1036 to 1204 | Copper Brazing |
| Metals -- Maximum Operation Temperatures | ||||
| Low Carbon Steel 1008-1015 | 800 deg. F | S. S. type 310 - 18-22 Ni - 24/26 Chrome | 1900 deg. F | |
| High Carbon Steel 1051 | 1050 deg. F | S. S. type 330 - 35 Ni - 15 Chrome | 1900 deg. F | |
| Monel -- 67 Ni - 30 Cu | 1000 deg. F | Incoloy - 35 Ni - 18 Chrome | 1900 deg. F | |
| S. S. type 410 12-14 Ch | 1400 deg. F | Inconel -80 Ni 13 Chrome | 2100 deg. F | |
| S. S. type 304 18 Ch 8 Ni | 1600 deg. F | Nichrome V - 80 Ni 20 Chrome | 2100 deg. F | |